Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 190 °C @Load 1.00 kg |
374 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 6005 PC/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 190 °C @Load 1.00 kg |
374 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 6005B PC/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 190 °C @Load 1.00 kg |
374 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 6005B UV PC/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 190 °C @Load 0.999 kg |
374 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi.. |
|||
Vicat Softening Point | 190 °C @Load 0.999 kg |
374 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation .. |