Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 50.0 - 170 °C | 122 - 338 °F | Average value: 93.4 °C Grade Count:212 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Maximum Service Temperature, Air | 110 - 170 °C | 230 - 338 °F | Average value: 159 °C Grade Count:6 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Maximum Service Temperature, Air | 160 - 170 °C | 320 - 338 °F | UL RTI |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |