Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 500 °C | 932 °F | Continuous |
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Oxidation threshold |
Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Continuous |
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Continuous |
Pyrotek NAD-500 Electrical Insulation Product Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Thermal Tolerance |
MarkeTech Silica Aerogel Silica aerogels are generally known for being an extremely lightweight transparent solid down to |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
Specialty Materials Boron Monofilament Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Short Term, depends on temperature gradient |
Schott BOROFLOAT® Borosilicate Float Glass This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro.. |
|||
Maximum Service Temperature, Air | 500 - 600 °C | 932 - 1110 °F | Continuous |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | No Load |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | No Load |
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
Eifeler Coatings Technology TiC/TiN CVD Coating The titanium carbide/titanium nitride combination layer is a standard layer well-proven over a long time. Layer properties: Very high hardness; Very good adhesion; Sufficient toughnessInforma.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
Eifeler Coatings Technology TiN PVD Coating Key Characteristics: standard all purpose coatingPrimary Applications: machining / cutting of iron based material; metal forming; plastic molding of highly abrasive plastics; orthopedic instrumentat.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | limited |
Chosun Refractories APC-50 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | limited |
Chosun Refractories APC-50G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | limited |
Chosun Refractories INCT-50S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Operating Temperature |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Operating Temperature |
California Fine Wire Nickel 271 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | Operating Temperature |
California Fine Wire Nickel 272 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating Metal-doped Me/a-C:H/a-Si:O nanocomposite. The electrical characteristics of these coatings can be tailored by the addition of metal dopants. This creates an engineered surface for specialized ap.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
BASF Sicotan® Yellow L 1010 Color Additive Description: Mixed-phase pigment with maximum fastness properties; Suitable for all coatings systems.Chemical Structure: Ni/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyan.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
BASF Sicotan® Yellow L 1012 Color Additive Description: Mixed-phase pigment with maximum fastness properties; Suitable for all coatings systems.Chemical Structure: Ni/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyan.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
BASF Sicotan® Yellow L 1910 Color Additive Description: Mixed-phase pigment with maximum fastness properties. Suitable for all coatings systemsChemical Structure: Cr/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyana.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
BASF Sicotan® Yellow L 1912 Color Additive Description: Mixed-phase pigment with maximum fastness properties. Suitable for all coatings systemsChemical Structure: Cr/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyana.. |
|||
Maximum Service Temperature, Air | 500 °C | 932 °F | |
Elisto THERMOSTAR® LD 500 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |