Polymer Property : Maximum Service Temperature, Air = 599 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 315 °C
599 °F
Pyrotek NAD-250 Structural Insulation Board
NAD-250 is a general purpose cement board. It is suitable for low-voltage electrical insulation in dry conditions.ApplicationsOven shelves Platen insulators Coil boxes Foundry core plates Heat guar..
Maximum Service Temperature, Air 315 °C
599 °F
Pyrotek S-2 Fabric
Coarse fabric with low air permeability. Excellent mechanical strength and abrasion resistance.Information provided by Pyrotek.
Maximum Service Temperature, Air 315 °C
599 °F
Continuous
Pyrotek TS-550 Insulating Board
TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the form..
Maximum Service Temperature, Air 315 °C
599 °F
Intermittent
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Maximum Service Temperature, Air 315 °C
599 °F
Intermittent
Momentive Performance Materials RTV116 One Component Acetoxy Adhesive Sealant, Red
RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. ..
Maximum Service Temperature, Air 315 °C
599 °F
Intermittent
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red
RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15..
Maximum Service Temperature, Air 315 °C
599 °F
Intermittent
Momentive Performance Materials RTV560 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, Red
RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand..
Maximum Service Temperature, Air 315 °C
599 °F
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Maximum Service Temperature, Air 315 °C
599 °F
Shin-Etsu Silicones KE-7021U Temperature Resistant Silicone Elastomer
KE7021 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 315 °C (67 ~ +600 °F)Typ..
Maximum Service Temperature, Air 315 °C
599 °F
for 1 hr
3M 7260M High Temperature Over Spray Protective Bags and Sheets
3M™ High Temperature Over Spray Protective Bags and Sheets 7260M are used for masking where high temperature resistance or custom sizes are needed. This high performance product is designed for mas..
Maximum Service Temperature, Air 315 °C
599 °F
3M Dyneon™ PFE 133TBZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 133TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F..
Maximum Service Temperature, Air 315 °C
599 °F
3M Dyneon™ 131TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ 131TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per AST..
Maximum Service Temperature, Air 315 °C
599 °F
3M Dyneon™ 81TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 81TZ is a technically advanced high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per ..
Maximum Service Temperature, Air 315 °C
599 °F
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per ..
Maximum Service Temperature, Air 315 °C
599 °F
3M Dyneon™ PFE 132TBZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 132TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F..
Maximum Service Temperature, Air 315 °C
599 °F
3M Dyneon™ PFE 191TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 81TZ, PFE 131TZ and PFE 191TZ are technically advanced high temperature perfluorelastomers (HT PFE). They are designed to meet the challenges of higher temperature applications. Th..