Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer
Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se..
Maximum Service Temperature, Air 177 °C
351 °F
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer
Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se..
Maximum Service Temperature, Air 177 °C
351 °F
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by ..
Maximum Service Temperature, Air 177 °C
351 °F
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Maximum Service Temperature, Air 177 °C
351 °F
Parker Chomerics Tecknit SC-Consil® 862 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol EA 9658 Film Adhesive
High temperature and high durability film adhesive designed for high toughness and high temperature performanceApplications: Composite Bonding Metal and Honeycomb Bonding
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol MA 562S Core Splice Adhesive
Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Nonmetallic, medium tack, excellent slump resistance.
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol PL 737 Film Adhesive
Nonmetallic, modified epoxy film specifically designed for use in structural aircraft components. Low flow characteristics.Application: Metal and Honeycomb Bonding
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol MA 557 Core Splice Adhesive
Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Designed to seal, splice or reinforce honeycomb materials. Excellent slump resistance, medium tack, n..
Maximum Service Temperature, Air 177 °C
351 °F
Specialty Materials 5521 Boron Epoxy Prepreg Tape
Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,..
Maximum Service Temperature, Air 177 °C
351 °F
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape
Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil..
Maximum Service Temperature, Air 177 °C
351 °F
Dow Corning 737 NEUTRAL CURE SEALANT
RTV adhesive/sealant with primerless adhesion to most materialsInformation provided by Dow Corning
Maximum Service Temperature, Air 177 °C
351 °F
ChevronTexaco NLGI 2 Moly MAX Grease EP
FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth ..
Maximum Service Temperature, Air 177 °C
351 °F
See Note 2.
ChevronTexaco Polystar® CVJ
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
Maximum Service Temperature, Air 177 °C
351 °F
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP
FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,..
Maximum Service Temperature, Air 177 °C
351 °F
ChevronTexaco NLGI 2 SRI Grease OEM
FeaturesChevron SRI Grease OEM is a high temperature ball and roller bearing grease.It is formulated with ISOSYN™ base stocks, a synthetic polyurea ashless organic thickener, and high performance ..
Maximum Service Temperature, Air 177 °C
351 °F
See Note 2.
ChevronTexaco Starplex® Moly NLGI Grade 2
Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh..
Maximum Service Temperature, Air 177 °C
351 °F
See Note 2.
ChevronTexaco Starplex® NLGI Grade 1
Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio..
Maximum Service Temperature, Air 177 °C
351 °F
3M 1675 Polyester Protective Tape
3M™ Polyester Protection Tape 1675 is a polyester tape with a low-tack adhesive system for temporary surface protection.Information provided by 3M
Maximum Service Temperature, Air 177 °C
351 °F
Short term
3M 9500B Double Coated Tapes with Adhesive 350
3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a ..
Maximum Service Temperature, Air 177 °C
351 °F
3M Scotch® 214 High-Temperature Masking Tape
Scotch® High Temperature Masking Tape 214 is good for one hour at 350°F (177°C) on most surfaces. The adhesive is sulfur-free which makes it one of the few tapes that can be used on copper, silve..
Maximum Service Temperature, Air 177 °C
351 °F
Long term
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Maximum Service Temperature, Air 177 °C
351 °F
Short term
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Maximum Service Temperature, Air 177 °C
351 °F
Short term
3M 9593 Double Coated Tapes with Adhesive 350
3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a ..
Maximum Service Temperature, Air 177 °C
351 °F
Short term
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints...
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol EA 9845 SF Composite Surfacing Film
Epoxy-based composite surfacing film improves surface quality of honeycomb stiffened composite parts. Reduced weight vs conventional surfacing films. Cures at 250°F/121°C or 350°F/177°C with a v..
Maximum Service Temperature, Air >= 177 °C
>= 351 °F
Henkel Hysol EA 9390 Paste Adhesive System
Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol EA 9825 Paste Adhesive System
Low-density, one-component epoxy syntactic for use on honeycomb composite parts requiring high compressive strength at temperatures up to 350°F / 177°C. Ideal for fastener or attachment potting an..
Maximum Service Temperature, Air 177 °C
351 °F
Henkel Hysol MA 562SFR Core Splice Adhesive
Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Flame-retardant, nonmetallic, medium tack, excellent slump resistance.