Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.875 - 3.125 g/cc
1.875 - 3.125 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 55
45 - 55
ASTM D2240
Tensile Strength >= 0.689 MPa
>= 100 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0060 ohm-cm
<= 0.0060 ohm-cm
Shielding Effectiveness >= 70 dB

@Frequency 100000 Hz
>= 70 dB

@Frequency 100000 Hz
H-Field
90 dB

@Frequency 1.00e+10 Hz
90 dB

@Frequency 1.00e+10 Hz
Plane Wave
>= 100 dB

@Frequency 1.00e+9 Hz
>= 100 dB

@Frequency 1.00e+9 Hz
Plane Wave
>= 130 dB

@Frequency 1.00e+7 Hz
>= 130 dB

@Frequency 1.00e+7 Hz
E-Field
Descriptive Properties Value Comments
Binder Silicone
Color Silver-Tan
Filler Pure Silver