ChevronTexaco Polystar® CVJ

Category Fluid , Lubricant , Urea Gellant
Manufacturer ChevronTexaco Corp
Trade Name Polystar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Polystar® CVJ.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.Base oilUnknown amount of work.CPS Number: 222013; MSDS Number: 8659
Physical Properties Metric English Comments
Viscosity Measurement 96
96
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 620 SUS
620 SUS
See Note 3.
Saybolt Viscosity at 210°F 69.5 SUS
69.5 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 118 cSt
118 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 12.5 cSt
12.5 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 57
57
Four Ball Wear 0.600 mm
0.0236 in
Scar Diameter
Penetration 160
160
Cold test, 6h, See Note 4.
Penetration P(60), 1/10 mm 312
312
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
See Note 2.
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
See Note 1.
Dropping Point 243 °C
469 °F
Descriptive Properties Value Comments
Bearing Rust Protection Pass
Color Cream
Texture Smooth
Thickener, % 11.5
Polyurea