Polymer Property : Maximum Service Temperature, Air = 2730 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1500 °C
2730 °F
Continuous
Pyrotek O'-Sialon Non-Oxide Ceramic
O'-Sialon is a unique class of non-oxide ceramic which incorporates grains of silicon carbide held by a matrix of O'-Sialon. This results in a product that exhibits high strength at both ..
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast ADHESIET 150 Dry Air-Setting Refractory Mortar
Description: Adhesiet 150 is an air setting mortar with a sodium silicate bond and is supplied as a dry powder. Because of the special mix of the raw materials it can be used up to 1500°C.Remarks..
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast ADHESIET 170 P Al Dry Air-Setting Refractory Mortar
Description: Adhesiet 170 P Al is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum meltin..
Maximum Service Temperature, Air 1500 °C
2730 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 42 Dense Refractory Brick
Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c..
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo..
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Maximum Service Temperature, Air 1500 °C
2730 °F
Misumi Alumina 99 Aluminum Oxide, Al2O3
Information provided by MISUMI Corporation.
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast CURON 150 GM Dense Refractory Castable
Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro..
Maximum Service Temperature, Air 1500 °C
2730 °F
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..
Maximum Service Temperature, Air 1500 °C
2730 °F
Sharadaa Ceramics HF 60 AL Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1500 °C
2730 °F
Sharadaa Ceramics LI SILL-I High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Maximum Service Temperature, Air 1500 °C
2730 °F
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables
Information provided by Sharadaa Ceramics Pvt. Ltd.
Maximum Service Temperature, Air 1500 °C
2730 °F
Stellar Canada CERAMITE® CSA Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..
Maximum Service Temperature, Air 1500 °C
2730 °F
Sharadaa Ceramics REFCAST C High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Maximum Service Temperature, Air 1500 °C
2730 °F
Sharadaa Ceramics VELCRETE G 401 Gunning Castables
Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling ..
Maximum Service Temperature, Air 1500 °C
2730 °F
Sharadaa Ceramics ZAP 011 Smart Cast Application
Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd.
Maximum Service Temperature, Air 1500 °C
2730 °F
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
DN 70 is a ZTA Alumina Toughened Zirconia.
Maximum Service Temperature, Air 1500 °C
2730 °F
Continuous
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Maximum Service Temperature, Air 1500 °C
2730 °F
NO-LOAD COND.
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia
Oxygen ionic conductor for extreme-stress and extreme-thermal-shock environments
Maximum Service Temperature, Air 1500 °C
2730 °F
No Load
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Maximum Service Temperature, Air 1500 °C
2730 °F
No Load
CoorsTek Zirconia-Toughened Alumina, ZTA
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Maximum Service Temperature, Air 1500 °C
2730 °F
Chosun Refractories 1500 ACE PAPER Paper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1500 °C
2730 °F
COI Ceramics Al2O3SiO2 Oxide Hollow Spheres
Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres tha..
Maximum Service Temperature, Air 1500 °C
2730 °F
limited
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1500 °C
2730 °F
Continuous
Zircar Ceramics AL-30AA Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Maximum Service Temperature, Air 1500 °C
2730 °F
Continuous
Zircar Ceramics ALCAA Alumina Insulation
ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics.
Maximum Service Temperature, Air 1500 °C
2730 °F
CeramTec AT 79 Alumina, 99.6%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Maximum Service Temperature, Air >= 1500 °C
>= 2730 °F
China-Yixing Longly Refractories 95 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..