Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Dry Air |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | for Continuous use with specialty cloth exterior or flexible core |
Pyrotek MT-29P Microporous Panel Insulation MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel.Applica.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Pyrotek Thermollite Insulating Refractory Shapes for Molten Aluminum Thermollite has been specifically developed for direct contact with molten aluminum and its various alloys. Thermollite provides the specific advantage of reducing heat loss in melt transfer applic.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | for Continuous use with specialty cloth exterior or flexible core |
Pyrotek MT-29L Microporous Ladle Lining Insulation MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Pyrotek NAD-1000 High Temperature Engineering Board NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | for long term exposure |
Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof Microtherm Marineguard® is a lightweight flexible overstitched panel of high performance thermal insulation designed to form easily around complex shapes for optimized protection. The panels are .. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | resists oxidation |
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | resists oxidation |
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Sinotek Materials BG Board Ceramic Fiber Board, White, Heat Insulation Material Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Skamol Group Moler M-EXTRA 'E' Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | No Load |
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Safe Operating Temp |
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | Safe Operating Temp |
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | limited |
Chosun Refractories GUN-100L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | limited |
Chosun Refractories INCT-100N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | limited |
Chosun Refractories INCT-100S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | limited |
Chosun Refractories MIX-2 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | no load |
Accuratus MACOR Machinable Glass Ceramic Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Gouda Vuurvast CURON 100 C Dense Refractory Castable Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values .. |
|||
Maximum Service Temperature, Air | 1000 °C | 1830 °F | |
Elisto THERMOSTAR® LD 1000 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |