| Category | Ceramic | 
| Manufacturer | Pyrotek, Inc. | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Pyrotek MT-29P Microporous Panel Insulation.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | <= 0.288 g/cc | <= 0.0104 lb/in³ | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Compressive Strength | 0.200 MPa | 29.0 psi | to 10% deformation | 
| 0.600 MPa | 87.0 psi | to 20% deformation | |
| 1.10 MPa | 160 psi | to 30% deformation | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Thermal Conductivity |           0.0290           W/m-K           @Temperature 260 °C  | 
                  0.201           BTU-in/hr-ft²-°F           @Temperature 500 °F  | 
        (Standard and Hydrophobic) | 
|           0.0420           W/m-K           @Temperature 537 °C  | 
                  0.291           BTU-in/hr-ft²-°F           @Temperature 999 °F  | 
        Standard | |
|           0.0480           W/m-K           @Temperature 537 °C  | 
                  0.333           BTU-in/hr-ft²-°F           @Temperature 999 °F  | 
        (Hydrophobic) | |
|           0.0490           W/m-K           @Temperature 649 °C  | 
                  0.340           BTU-in/hr-ft²-°F           @Temperature 1200 °F  | 
        Standard | |
|           0.0560           W/m-K           @Temperature 649 °C  | 
                  0.389           BTU-in/hr-ft²-°F           @Temperature 1200 °F  | 
        Hydrophobic | |
| Maximum Service Temperature, Air | 650 °C | 1200 °F | for Continuous use with standard cloth exterior | 
| 1000 °C | 1830 °F | for Continuous use with specialty cloth exterior or flexible core | |
| Shrinkage |           0.300 %                     @Temperature 538 °C, Time 86400 sec  | 
                  0.300 %                     @Temperature 1000 °F, Time 24.0 hour  | 
        |
|           0.600 %                     @Temperature 815 °C, Time 86400 sec  | 
                  0.600 %                     @Temperature 1500 °F, Time 24.0 hour  | 
        ||
|           1.00 %                     @Temperature 954 °C, Time 86400 sec  | 
                  1.00 %                     @Temperature 1750 °F, Time 24.0 hour  |