Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite Optix® CP - 41 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 50.0 - 170 °C | 122 - 338 °F | Average value: 93.4 °C Grade Count:212 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite West Optix® CP - 41 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | UL-746 ABC |
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-65 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-75C Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-85 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-90 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9077-90 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 916V0-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9604-80C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | RTI |
Sylvin Technologies 9604-95 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Application; ASTM C1299 |
3M IC 15WB+ Fire Barrier Sealant 3M Fire Barrier Sealant IC 15WB+ is a cost-effective, one-part, gun-grade, latex-based, intumescent firestop sealant that dries to form a monolithic firestop seal that also acts as a barrier to airb.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
Abatron 8509-2A/8509-1B Carbon-Filled Electrically Conductive Epoxy Compound 8509-2A/8509-1B is a solventless carbon-epoxy system used as an adhesive and silk-screening material with anti-static and other lower-conductivity requirements. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
Abatron 8509-3 A/B Carbon-Filled Electrically Conductive Epoxy Compound 8509-3 A/B is a solventless carbon-epoxy system used as an adhesive and silk-screening material with anti-static and other lower-conductivity requirements. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
Abatron 8509-4 A/B Carbon-Filled Electrically Conductive Epoxy Compound 8509-4 A/B is a solventless carbon-epoxy system used as an adhesive and silk-screening material with anti-static and other lower-conductivity requirements. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Deflection Temp at unknown load |
Abatron AboCast 7703-21/AboCure 7703-24 (D) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Deflection Temp at unknown load |
Abatron AboCast 8503-5/AboCure 8503-5 Colorless Epoxy AboCast 8503-5/AboCure 8503-5 is a faster hardening, colorless epoxy casting compound used for small castings and decoupage. It is a good choice for small castings, especially for analytical purpose.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | Application; ASTM C1299 |
3M FD 150+ Fire Barrier Sealant 3M Fire Barrier Sealant FD 150+ is an economical, ready to use, gun-grade, elastomeric sealant that dries to from a monolithic flexible firestop seal. 3M Fire Barrier Sealant FD 150+ firestops joint.. |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | White |
3M Scotchkote™ 80XRG 539 Urethane Elastomer Scotchkote Urethane Elastomer 80XRG 539 has been specifically developed as a fast curing elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components... |
|||
Maximum Service Temperature, Air | 50.0 °C | 122 °F | |
3M SS100 Smoke and Sound Sealant 3M Smoke and Sound Sealant SS 100 is an economical, ready to use, gun-grade, elastomeric sealant that drives to form a monolithic flexible seal that helps prevent unwanted noise infiltration and mit.. |