Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 1110 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 600 °C
1110 °F
Continuous
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite
Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m..
Maximum Service Temperature, Air 600 °C
1110 °F
Oxidation Resistance
Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
Maximum Service Temperature, Air 600 °C
1110 °F
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si)
Features: A near alpha, high temperature creep resistant alloy developed for elevated temperature use in the range of 600°C that offers the highest combination of strength, creep resistance, fractu..
Maximum Service Temperature, Air 600 °C
1110 °F
Eifeler Coatings Technology CrCN PVD Coating
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal..
Maximum Service Temperature, Air 600 °C
1110 °F
Eifeler Coatings Technology CrN PVD Coating
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal..
Maximum Service Temperature, Air 600 °C
1110 °F
Eifeler Coatings Technology ZrCN PVD Coating
Key Characteristics: decorative color, good wear and corrosion resistancePrimary Applications: machining of cast aluminum, brass, copper, bronze, non-alloyed aluminum; machining of fiberglass, nylon..
Maximum Service Temperature, Air 600 °C
1110 °F
Chosun Refractories AH-3 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 600 °C
1110 °F
Elisto THERMOSTAR® LC 400 GL Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto
Maximum Service Temperature, Air 600 °C
1110 °F
Operating Temperature
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Maximum Service Temperature, Air 600 °C
1110 °F
3M H50/10000EPX Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M iM30K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M K1 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M K15 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M K20 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M K37 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M K46 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S32 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S35 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S38 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S60HS Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
Beijing Evergrow Resources GFF-10 Glass Fiber Felt
Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a..
Maximum Service Temperature, Air 600 °C
1110 °F
Beijing Evergrow Resources GFF-3 Glass Fiber Felt
Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a..
Maximum Service Temperature, Air 600 °C
1110 °F
3M K25 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S15 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S38HS Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M S60 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
3M D32/4500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Maximum Service Temperature, Air 600 °C
1110 °F
Oxidation Resistance
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
Maximum Service Temperature, Air 600 °C
1110 °F
Beijing Evergrow Resources GFF-5 Glass Fiber Felt
Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a..