Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M iM30K Glass Bubbles

Category Ceramic , Glass
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M iM30K Glass Bubbles.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding applications. These low-density particles are used in a wide range of industries to reduce part weight, lower costs and enhance product properties. The unique spherical shape of 3M glass bubbles offers a number of important benefits, including: higher filler loading, lower viscosity/improved flow and reduced shrinkage and warpage. It also helps the 3M glass bubbles blend readily into compounds and makes them adaptable to a variety of production processes including spraying, casting and molding. The chemically stable soda-lime-borosilicate glass composition of 3M glass bubbles provides excellent water resistance to create more stable emulsions. They are also non-combustible and nonporous, so they do not absorb resin. And, their low alkalinity gives 3M glass bubbles compatibility with most resins, stable viscosity and long shelf life.Information provided by 3M
Physical Properties Metric English Comments
Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
0.600 g/cc
0.0217 lb/in³
Volatiles 0.50 %
0.50 %
Particle Size 8.6 µm
8.6 µm
10th%
15.3 µm
15.3 µm
50th%
23.6 µm
23.6 µm
90th%
26.7 µm
26.7 µm
Effective Top Size
Mechanical Properties Metric English Comments
Compressive Strength 193 MPa
28000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 600 °C
1110 °F
Electrical Properties Metric English Comments
Dielectric Constant 1.2 - 1.7

@Frequency 1.00e+8 Hz
1.2 - 1.7

@Frequency 1.00e+8 Hz
Descriptive Properties Value Comments
Alkalinity <0.5 milliequivalents/gram
Appearance White
unaided eye
Chemical Resistance soda-lime-borosilicate glass
Oil Absorption 0.2-0.6 g oil/100 cc