Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 540 °C | 1000 °F | |
Pyrotek Jacketed mesh core Tadpoles 304 stainless steel mesh core with continuous fiberglass jacket. Excellent where no mounting flange is required.AdvantagesGood Abrasion Resistance Excellent Compression and Recall Information provi.. |
|||
Maximum Service Temperature, Air | 540 °C | 1000 °F | |
Pyrotek R-3C Silicone Coated Rope R-3 rope with silicone coating to increase abrasion resistance and air sealing properties.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Continuous |
Pyrotek TS-450 Thermoset Electrical Insulation Product Glass reinforcement, Mica resin, Silver color. Highest temperature resistance. High dielectric properties.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 540 °C | 1000 °F | |
Pyrotek A-1 Glass Fiber Core Rope Compressible, inexpensive rope. Glass fiber core with heavy gauge glass fabric jacket. Loses tensile strength after 340°C but remains intact.AdvantagesGood Abrasion Resistance Good Compression an.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steamThermally stable fibers retain effective seal even during thermal .. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF17 Industrial Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF17 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF37 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF45 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® SF60 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Fabric Limit, Continuous |
Mid-Mountain Materials ARMATEX® FF18 Fluoroelastomer Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Maximum Service Temperature, Air | 540 °C | 1000 °F | Intermittent |
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
Maximum Service Temperature, Air | 540 °C | 1000 °F | Intermittent |
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2) Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,.. |
|||
Maximum Service Temperature, Air | 540 °C | 1000 °F | Good creep resistance |
TIMET TIMETAL® 829 (Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si) Titanium Alloy Weldable, High Strength, High Temperature, Creep Resistant AlloyFeatures: TIMETAL 829 combines creep resistance up to 540°C with good oxidation resistance. It is weldable and like TIMETAL 685, TIME.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Chesterton 787 Sliding Paste Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate Good thermal and dielectric properties and can be fired to increase temperature resistance and mechanical strength. Easily machined to close tolerances. Plates, rods and bars available to 12". |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Long Term |
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C). |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
PSM Industries Ferro-TiC® CHW-25 Hot Work Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | |
PSM Industries Ferro-TiC® CHW-45 Hot Work Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Maximum Service Temperature, Air | 538 °C | 1000 °F | Ductility maintained well above this temp. |
ATI Allegheny Ludlum AL 825™ Nickel Alloy Allegheny Ludlum AL 825 alloy is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of corrosion resistance to both moderately oxidizing and moderately reducing enviro.. |