Pyrotek TS-450 Thermoset Electrical Insulation Product

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek TS-450 Thermoset Electrical Insulation Product.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Glass reinforcement, Mica resin, Silver color. Highest temperature resistance. High dielectric properties.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.098 g/cc
0.07580 lb/in³
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Flexural Strength 193 MPa
28000 psi
Compressive Strength 400 MPa
58000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 538 °C
1000 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 2.54e+16 ohm-cm
2.54e+16 ohm-cm
Dielectric Strength 17.0 kV/mm
432 kV/in
Arc Resistance 360 sec
360 sec