Polymer Property : Maximum Service Temperature, Air = 60.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.0 - 60.0 °C
104 - 140 °F
long term; EMS
EMS-Grivory Grivory® GTR 45 PA6I/6T
Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 007 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 019 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 022 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 025 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 027 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 029 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 032 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 036 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 042 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 047 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 049 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 057 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 089 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 3273 Standard SBS Thermoplastic Elastomer Compound
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 3275 Standard SBS Thermoplastic Elastomer Compound
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 003 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 068 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 075 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 076 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 081 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 084 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Maximum Service Temperature, Air 55.0 - 60.0 °C
131 - 140 °F
AlphaGary Evoprene™ 091 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..