Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.990 g/cc | 0.990 g/cc | ISO 2782 |
Viscosity Measurement | 17 @Temperature 150 °C |
17 @Temperature 302 °F |
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 28 | 28 | ISO 868 |
Tensile Strength | 4.40 MPa | 638 psi | ISO 37 |
Elongation at Break | 860 % | 860 % | ISO 37 |
100% Modulus | 0.000700 GPa | 0.102 ksi | ISO 37 |
Tear Strength | 18.0 kN/m | 103 pli | ISO 34-B |
Compression Set | 14 % @Temperature 22.0 °C, Time 259000 sec |
14 % @Temperature 71.6 °F, Time 72.0 hour |
ISO 815 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 55.0 - 60.0 °C | 131 - 140 °F | |
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Bonds with | Polystyrene | |
Chemical Resistance | Acetone | Moderate |
Acids up to 80% | Moderate | |
Alcohol | Good | |
Alkalis | Good | |
Brake fluid | Moderate | |
Chlorinate solvents | Poor | |
Diesel | Poor | |
Ethylene glycol | Excellent | |
Gasoline | Poor | |
Salt solution | Good | |
Soda lye | Moderate | |
Water, 23°C | Good | |
Water, 95°C | Poor | |
Ozone Resistance | Fail - Crack | 100 pphm / 200 hrs / 20% strain |
Transparency | Opaque |