Polymer Property : Maximum Service Temperature, Air = 300 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 - 300 °C
500 - 572 °F
Average value: 263 °C Grade Count:12
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min..
Maximum Service Temperature, Air 260 - 300 °C
500 - 572 °F
Average value: 264 °C Grade Count:17
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Maximum Service Temperature, Air 150 - 300 °C
302 - 572 °F
Average value: 215 °C Grade Count:36
Overview of materials for Silicone, RTV, Encapsulation Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2513S-20-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2514S-10-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2515S-10-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2515S-20-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2515S-30-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2516S-20-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2516S-30-10 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2518S-10-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2518S-20-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2518S-40-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2519S-40-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2521S-40-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2521S-50-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2521S-60-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 25235-50-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 25235-60-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2524S-20-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh envi..
Maximum Service Temperature, Air 150 - 300 °C

@Pressure 0.000 - 10.0 MPa
302 - 572 °F

@Pressure 0.000 - 1450 psi
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate
Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru..
Maximum Service Temperature, Air 150 - 300 °C

@Pressure 0.000 - 5.00 MPa
302 - 572 °F

@Pressure 0.000 - 725 psi
Recommended Application Range
Arlon UltraPad™ 51073G031D Silicone-Based Press Pad
Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data..
Maximum Service Temperature, Air 150 - 300 °C

@Pressure 0.000 - 5.00 MPa
302 - 572 °F

@Pressure 0.000 - 725 psi
Recommended Application Range
Arlon UltraPad™ 51073R031D Silicone-Based Press Pad
UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre..
Maximum Service Temperature, Air 100 - 300 °C

@Pressure 0.000 - 10.0 MPa
212 - 572 °F

@Pressure 0.000 - 1450 psi
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish"
Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio..
Maximum Service Temperature, Air 98.0 - 300 °C
208 - 572 °F
Average value: 227 °C Grade Count:6
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2519S-20-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2519S-50-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2521S-30-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 25235-40-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro..
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
SMAC CABLE® 2525S-30-08 Damping Material
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh enviro..