Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
Pyrotek Pyroboard™ S1000 Roller Pyroboard™ S1000 is designed to be used throughout the preheat and cooling sections of the furnace.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
PSM Industries Ferro-TiC® HT-6A Age Hardenable Nickel Base Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Base Fabric, Continuous |
Mid-Mountain Materials ARMATEX® SRS 28 Silica Fabric Coated with Silicone Rubber ARMATEX® SRS 28 is a silica fabric coated with silicone rubber on one or both sides to a finished weight of 28 oz/sq yd. An ideal product for heavy duty protection of equipment and personnel, ARM.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Base Fabric, Continuous |
Mid-Mountain Materials ARMATEX® SRS 40 Silica Fabric Impregnated with Silicone Rubber ARMATEX® SRS 40 is a silica fabric impregnated with silicone rubber on one side to a finished weight of 40 oz/sq yd. An ideal product for heavy duty protection of equipment and personnel. ARMATEX.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Mid-Mountain Materials SILTEX® XS-150 Silica Yarn SILTEX® SILICA YARN XS-150 is comprised of continuous filament, amorphous silica fibers and offers superior protection in electrical applications, as well as excellent resistance to thermal shock.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® FC-25 Tamping Mix Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Vari-Form™ B Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Continuous |
Unifrax Foamfrax® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
Universal Wire Works No. 1 Cobalt Alloy Welding Wire Universal No. 1 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme abrasion resistance at elevated temperatures. Excellent for resistance to corrosion and oxidation where .. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Duraback® Ceramic Fiber Insulator Fiberfrax Duraback blanket is a strong, lightweight, flexible needled blanket intended for use as a cost-effective back-up insulation in Fiberwall® furnace linings. It is recommended for use up to.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Scaling Temperature for Continuous Service |
Carpenter Gall-Tough PLUS™ Stainless, Annealed Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Scaling Temperature for Continuous Service |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | oxidation resistance to this temp |
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | |
BNZ Materials 508 Insulating Cement 508 Insulating Cement is an 1800°F service product, utilized in the refractory applications requiring a combination of insulating value and high temperature performance. Typical Applications: Insul.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Scaling Temperature for Continuous Service |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Maximum Service Temperature, Air | 982 °C | 1800 °F | Scaling Temperature for Continuous Service |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |