Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 800 °C | 1470 °F | Dry Air |
Outokumpu 4713 High Temperature Ferritic Stainless Steel Does not form brittle phases but should only be exposed to moderately corrosive atmospheres due to low chromium content.Applications: Mostly used in high temperature applications with sulphurous atm.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | Dry Air |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | Continuous |
Pyrotek Pyrite B-3 Refractory Board Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | oxidation limit |
Momentive Performance Materials Niobium Carbide (NbC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | oxidation limit |
Momentive Performance Materials Zirconium Carbide (ZrC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Sharadaa Ceramics REFCAST LT Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Sharadaa Ceramics Resin Bonded Slabs Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | continuous, glass fabric |
Unifrax Excelfrax® 1900 Panel Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | No load condition |
CoorsTek Hot Pressed Aluminum Nitride Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors H.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | Continuous |
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Eifeler Coatings Technology EXXTRAL® plus PVD Coating Key Characteristics: high hardness, very good oxidation resistance, low thermal conductivityPrimary Applications: machining of hardened steel and thicker steel sheets; excellent chemical resistance;.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Eifeler Coatings Technology EXXTRAL® rose PVD Coating Key Characteristics: high hardness and elasticity, low friction, high oxidation resistancePrimary Applications: excellent for stainless steel and nickel-based high temperature alloys; hard and copy .. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Eifeler Coatings Technology EXXTRAL® silver PVD Coating Key Characteristics: high hardness, good oxidation resistance, low frictionPrimary Applications: machining of abrasive or sticking materials (stainless steel, cast iron, Si-rich Al-alloys); machinin.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Eifeler Coatings Technology VARIANTA® TiAlN PVD Coating Key Characteristics: high hardness, very good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of cast iron and nickel base.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Eifeler Coatings Technology VARIANTIC® TiAlCN PVD Coating Key Characteristics: low friction, good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of all types of steel under dry as.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Chosun Refractories AH-4 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | limited |
Chosun Refractories APC-80 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | limited |
Chosun Refractories APC-80G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | limited |
Chosun Refractories GUN-80L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | limited |
Chosun Refractories INCT-80N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | limited |
Chosun Refractories INCT-80S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | |
Elisto THERMOSTAR® HD 800 Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | Operating Temperature |
California Fine Wire Nickel Alloy 90 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | oxidation limit |
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr.. |
|||
Maximum Service Temperature, Air | 800 °C | 1470 °F | Dry Air |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |