Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 700 °C | 1290 °F | Continuous |
Pyrotek F-51 Dense Machinable Board F-51 is a high temperature resin base, supplemented with fiberglass and graphite to provide extra strength and lubricity. F-51 is abrasion resistant and suitable for hot glass handling applications.. |
|||
Maximum Service Temperature, Air | 700 °C | 1290 °F | oxidation limit |
Momentive Performance Materials Tantalum Carbide (TaC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Maximum Service Temperature, Air | 700 °C | 1290 °F | |
MetalTek MTEK 27-5 Cast UNS J93015 Heat Resistant Stainless Steel Higher nickel yields improved strength. Resists high sulfur process gas.Applications: Pour spouts, holding pots, kiln parts, gas parts.Information provided by MetalTek |
|||
Maximum Service Temperature, Air | 700 °C | 1290 °F | 100 to 10,000 hr, depends on temperature gradient |
Schott Dark ROBAX® Glass Ceramic Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolle.. |
|||
Maximum Service Temperature, Air | 700 °C | 1290 °F | |
Sharadaa Ceramics Resin Bonded Mattresses Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 700 °C | 1290 °F | good strength and oxidation resistance |
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy Data provided by the manufacturer, Special Metals. |
|||
Maximum Service Temperature, Air | 700 °C | 1290 °F | |
Eifeler Coatings Technology TOPMATIC TiAlN PVD Coating This layer on the basis of TiAlN is relatively tough and can therefore be deposited in comparably high layer thicknesses. The adhesion of the coating is outstanding.Information provided by Eifeler C.. |