| Category | Metal , Superalloy , Iron Base |
| Manufacturer | Special Metals (includes the former Inco Alloys International Inc.) |
| Trade Name | INCOLOY® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.94 g/cc | 0.287 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Elasticity | 201 GPa | 29200 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 16.4 µm/m-°C @Temperature 27.0 - 100 °C |
9.11 µin/in-°F @Temperature 80.6 - 212 °F |
Mean |
| 16.9 µm/m-°C @Temperature 27.0 - 300 °C |
9.39 µin/in-°F @Temperature 80.6 - 572 °F |
Mean | |
| 17.5 µm/m-°C @Temperature 27.0 - 500 °C |
9.72 µin/in-°F @Temperature 80.6 - 932 °F |
Mean | |
| 17.7 µm/m-°C @Temperature 27.0 - 700 °C |
9.83 µin/in-°F @Temperature 80.6 - 1290 °F |
Mean | |
| Specific Heat Capacity | 0.419 J/g-°C | 0.100 BTU/lb-°F | |
| Thermal Conductivity | 12.7 W/m-K | 88.1 BTU-in/hr-ft²-°F | |
| Melting Point | 1370 - 1430 °C | 2500 - 2610 °F | |
| Solidus | 1370 °C | 2500 °F | |
| Liquidus | 1430 °C | 2610 °F | |
| Maximum Service Temperature, Air | 700 °C | 1290 °F | good strength and oxidation resistance |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Aluminum, Al | <= 0.35 % | <= 0.35 % | |
| Boron, B | 0.0010 - 0.010 % | 0.0010 - 0.010 % | |
| Carbon, C | <= 0.080 % | <= 0.080 % | |
| Chromium, Cr | 13.5 - 16 % | 13.5 - 16 % | |
| Iron, Fe | 60 % | 60 % | As remainder |
| Manganese, Mn | <= 2.0 % | <= 2.0 % | |
| Molybdenum, Mo | 1.0 - 1.5 % | 1.0 - 1.5 % | |
| Nickel, Ni | 24 - 27 % | 24 - 27 % | |
| Sulfur, S | <= 0.030 % | <= 0.030 % | |
| Titanium, Ti | 1.9 - 2.35 % | 1.9 - 2.35 % | |
| Tungsten, W | 3.0 - 4.5 % | 3.0 - 4.5 % | |
| Vanadium, V | 0.10 - 0.50 % | 0.10 - 0.50 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000910 ohm-cm | 0.0000910 ohm-cm | |
| Magnetic Permeability | 1.007 | 1.007 | at 200 Oersted (15.9 kA/m) |