Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 600 °C | 1110 °F | Oxidation Resistance |
Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si) Features: A near alpha, high temperature creep resistant alloy developed for elevated temperature use in the range of 600°C that offers the highest combination of strength, creep resistance, fractu.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Continuous Use, with Glass Fiber Reinforcement |
Zircar Ceramics AS-1260 Alumina-Silica Textile Multiple forms of ceramic fiber textiles made of reinforced yarn. Amazingly strong, they are useful as gasketing, insulation and fire protection to temperatures of 1260°C (2300°F).Information pro.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Eifeler Coatings Technology CrCN PVD Coating Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Eifeler Coatings Technology CrN PVD Coating Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Eifeler Coatings Technology ZrCN PVD Coating Key Characteristics: decorative color, good wear and corrosion resistancePrimary Applications: machining of cast aluminum, brass, copper, bronze, non-alloyed aluminum; machining of fiberglass, nylon.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Elisto THERMOSTAR® LC 400 GL Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Operating Temperature |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M H50/10000EPX Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M iM16K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M iM30K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K37 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K46 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Beijing Evergrow Resources GFF-10 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
Beijing Evergrow Resources GFF-3 Glass Fiber Felt Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic a.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M S60 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Maximum Service Temperature, Air | 600 °C | 1110 °F | Oxidation Resistance |
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |