Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | <= 343 °C | <= 650 °F | max. recommended film temperature |
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong.. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | Fired Heaters |
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | fired heaters |
Paratherm Corporation Paratherm™ HT Heat Transfer Fluid Paratherm HT Heat Transfer Fluid is a partially hydrogenated terphenyl based product designed for closed-loop liquid phase heating to 650°F (343°C) in fired heaters and 675°F (358°C) in solid fu.. |
|||
Maximum Service Temperature, Air | 343 °C @Pressure 13.8 MPa |
650 °F @Pressure 2000 psi |
Continuous |
Garlock 9850 Compressed Carbon Fiber Gasketing, Nitrile Binder Carbon fibers with a nitrile binder.Carbon fiber gasketing excels in harshest conditions - intense heat, high pressure, saturated steam and hot oils.Laboratory-tested for fire safety.Long-lasting se.. |
|||
Maximum Service Temperature, Air | 343 °C @Pressure 13.8 MPa |
650 °F @Pressure 2000 psi |
Continuous |
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLo.. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | Continuous |
Mid-Mountain Materials HYTEX® 700 Kevlar® Glass Industrial Textile Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Maximum Service Temperature, Air | 343 °C @Pressure 13.8 MPa |
650 °F @Pressure 2000 psi |
Continuous |
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective se.. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | |
Cotronics Duralco™ 124 650°F (340°C) Silver Filled Epoxy Two component, silver-filled epoxy for hi-power applications. Cures with mild heat. |
|||
Maximum Service Temperature, Air | 343 °C | 650 °F | |
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |