Material Notes:
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers superior protection from fluid degradation. Duratherm S offers the ultimate in fluid protection and is best suited for applications not prone to contamination or leaking.Information provided by Duratherm.
Physical Properties Metric English Comments
Density 0.830 g/cc
<br>@Temperature 316 °C
0.0300 lb/in³
<br>@Temperature 600 °F
0.841 g/cc
<br>@Temperature 288 °C
0.0304 lb/in³
<br>@Temperature 550 °F
0.855 g/cc
<br>@Temperature 260 °C
0.0309 lb/in³
<br>@Temperature 500 °F
0.879 g/cc
<br>@Temperature 204 °C
0.0318 lb/in³
<br>@Temperature 400 °F
0.958 g/cc
<br>@Temperature 37.8 °C
0.0346 lb/in³
<br>@Temperature 100 °F
Kinematic Viscosity 3.37 cSt
<br>@Temperature 260 °C
3.37 cSt
<br>@Temperature 500 °F
3.92 cSt
<br>@Temperature 260 °C
3.92 cSt
<br>@Temperature 500 °F
4.46 cSt
<br>@Temperature 260 °C
4.46 cSt
<br>@Temperature 500 °F
Kinematic Viscosity at 40°C (104°F) 36.6 cSt
36.6 cSt
Kinematic Viscosity at 100°C (212°F) 16.1 cSt
16.1 cSt
Vapor Pressure 0.0124 bar
<br>@Temperature 204 °C
9.27 torr
<br>@Temperature 400 °F
0.0203 bar
<br>@Temperature 260 °C
15.2 torr
<br>@Temperature 500 °F
0.0203 bar
<br>@Temperature 288 °C
15.2 torr
<br>@Temperature 550 °F
0.06964 bar
<br>@Temperature 316 °C
52.23 torr
<br>@Temperature 600 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.69 J/g-°C
<br>@Temperature 37.8 °C
0.403 BTU/lb-°F
<br>@Temperature 100 °F
1.97 J/g-°C
<br>@Temperature 204 °C
0.472 BTU/lb-°F
<br>@Temperature 400 °F
2.07 J/g-°C
<br>@Temperature 260 °C
0.495 BTU/lb-°F
<br>@Temperature 500 °F
2.12 J/g-°C
<br>@Temperature 288 °C
0.507 BTU/lb-°F
<br>@Temperature 550 °F
2.17 J/g-°C
<br>@Temperature 316 °C
0.518 BTU/lb-°F
<br>@Temperature 600 °F
Thermal Conductivity 0.0726 W/m-K
<br>@Temperature 316 °C
0.504 BTU-in/hr-ft²-°F
<br>@Temperature 600 °F
0.0778 W/m-K
<br>@Temperature 288 °C
0.540 BTU-in/hr-ft²-°F
<br>@Temperature 550 °F
0.0830 W/m-K
<br>@Temperature 260 °C
0.576 BTU-in/hr-ft²-°F
<br>@Temperature 500 °F
0.0951 W/m-K
<br>@Temperature 204 °C
0.660 BTU-in/hr-ft²-°F
<br>@Temperature 400 °F
0.130 W/m-K
<br>@Temperature 37.8 °C
0.900 BTU-in/hr-ft²-°F
<br>@Temperature 100 °F
Maximum Service Temperature, Air 343 °C
650 °F
Pour Point -66.1 °C
-87.0 °F
Flammability Test 636
636
Fire Point, °F
818
818
Autoignition Temp, °F
Flash Point 324 °C
615 °F
Descriptive Properties Value Comments
Distillation range at 10% 922
Distillation Range at 90% 1255
Max Bulk Temp (°F) 650
Max Film Temp (°F) 700