Material Notes:
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and full convection heaters.ApplicationsGas processingChemical processesWaste oil recoveryBiodiesel productionPlastic processingInformation Provided by Paratherm Corporation
Physical Properties Metric English Comments
Density 0.689 g/cc

@Temperature 371 °C
0.0249 lb/in³

@Temperature 700 °F
0.737 g/cc

@Temperature 316 °C
0.0266 lb/in³

@Temperature 600 °F
0.769 g/cc

@Temperature 260 °C
0.0278 lb/in³

@Temperature 500 °F
0.817 g/cc

@Temperature 204 °C
0.0295 lb/in³

@Temperature 400 °F
0.865 g/cc

@Temperature 149 °C
0.0312 lb/in³

@Temperature 300 °F
0.897 g/cc

@Temperature 93.3 °C
0.0324 lb/in³

@Temperature 200 °F
0.945 g/cc

@Temperature 37.8 °C
0.0341 lb/in³

@Temperature 100 °F
0.993 g/cc

@Temperature -17.8 °C
0.0359 lb/in³

@Temperature 0.000 °F
Viscosity 0.32 cP

@Temperature 371 °C
0.32 cP

@Temperature 700 °F
0.34 cP

@Temperature 357 °C
0.34 cP

@Temperature 675 °F
0.36 cP

@Temperature 343 °C
0.36 cP

@Temperature 650 °F
0.38 cP

@Temperature 329 °C
0.38 cP

@Temperature 625 °F
0.41 cP

@Temperature 316 °C
0.41 cP

@Temperature 600 °F
0.44 cP

@Temperature 302 °C
0.44 cP

@Temperature 575 °F
0.47 cP

@Temperature 288 °C
0.47 cP

@Temperature 550 °F
0.50 cP

@Temperature 274 °C
0.50 cP

@Temperature 525 °F
0.54 cP

@Temperature 260 °C
0.54 cP

@Temperature 500 °F
0.59 cP

@Temperature 246 °C
0.59 cP

@Temperature 475 °F
0.64 cP

@Temperature 232 °C
0.64 cP

@Temperature 450 °F
0.71 cP

@Temperature 218 °C
0.71 cP

@Temperature 425 °F
0.78 cP

@Temperature 204 °C
0.78 cP

@Temperature 400 °F
0.87 cP

@Temperature 191 °C
0.87 cP

@Temperature 375 °F
0.98 cP

@Temperature 177 °C
0.98 cP

@Temperature 350 °F
1.1 cP

@Temperature 163 °C
1.1 cP

@Temperature 325 °F
1.3 cP

@Temperature 149 °C
1.3 cP

@Temperature 300 °F
1.5 cP

@Temperature 135 °C
1.5 cP

@Temperature 275 °F
1.8 cP

@Temperature 121 °C
1.8 cP

@Temperature 250 °F
2.1 cP

@Temperature 107 °C
2.1 cP

@Temperature 225 °F
2.6 cP

@Temperature 93.3 °C
2.6 cP

@Temperature 200 °F
3.8 cP

@Temperature 79.4 °C
3.8 cP

@Temperature 175 °F
5.1 cP

@Temperature 65.6 °C
5.1 cP

@Temperature 150 °F
7.9 cP

@Temperature 51.7 °C
7.9 cP

@Temperature 125 °F
12 cP

@Temperature 37.8 °C
12 cP

@Temperature 100 °F
22 cP

@Temperature 23.9 °C
22 cP

@Temperature 75.0 °F
52 cP

@Temperature 10.0 °C
52 cP

@Temperature 50.0 °F
133 cP

@Temperature -3.89 °C
133 cP

@Temperature 25.0 °F
546 cP

@Temperature -17.8 °C
546 cP

@Temperature 0.000 °F
Molecular Weight 240 g/mol
240 g/mol
Average
Vapor Pressure 0.00758 bar

@Temperature 163 °C
5.69 torr

@Temperature 325 °F
0.0338 bar

@Temperature 204 °C
25.4 torr

@Temperature 400 °F
0.117 bar

@Temperature 246 °C
87.8 torr

@Temperature 475 °F
0.345 bar

@Temperature 288 °C
259 torr

@Temperature 550 °F
0.896 bar

@Temperature 329 °C
672 torr

@Temperature 625 °F
2.00 bar

@Temperature 371 °C
1500 torr

@Temperature 700 °F
Thermal Properties Metric English Comments
CTE, linear 324 µm/m-°C
180 µin/in-°F
converted from volume expansion
Specific Heat Capacity 1.84 J/g-°C

@Temperature -17.8 °C
0.440 BTU/lb-°F

@Temperature 0.000 °F
1.97 J/g-°C

@Temperature 37.8 °C
0.470 BTU/lb-°F

@Temperature 100 °F
2.09 J/g-°C

@Temperature 93.3 °C
0.500 BTU/lb-°F

@Temperature 200 °F
2.22 J/g-°C

@Temperature 149 °C
0.530 BTU/lb-°F

@Temperature 300 °F
2.34 J/g-°C

@Temperature 204 °C
0.560 BTU/lb-°F

@Temperature 400 °F
2.47 J/g-°C

@Temperature 260 °C
0.590 BTU/lb-°F

@Temperature 500 °F
2.59 J/g-°C

@Temperature 316 °C
0.620 BTU/lb-°F

@Temperature 600 °F
2.72 J/g-°C

@Temperature 371 °C
0.650 BTU/lb-°F

@Temperature 700 °F
Thermal Conductivity 0.0813 W/m-K

@Temperature 371 °C
0.564 BTU-in/hr-ft²-°F

@Temperature 700 °F
0.0916 W/m-K

@Temperature 316 °C
0.636 BTU-in/hr-ft²-°F

@Temperature 600 °F
0.0986 W/m-K

@Temperature 260 °C
0.684 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.105 W/m-K

@Temperature 204 °C
0.732 BTU-in/hr-ft²-°F

@Temperature 400 °F
0.111 W/m-K

@Temperature 149 °C
0.768 BTU-in/hr-ft²-°F

@Temperature 300 °F
0.114 W/m-K

@Temperature 93.3 °C
0.792 BTU-in/hr-ft²-°F

@Temperature 200 °F
0.118 W/m-K

@Temperature -17.8 °C
0.816 BTU-in/hr-ft²-°F

@Temperature 0.000 °F
0.118 W/m-K

@Temperature 37.8 °C
0.816 BTU-in/hr-ft²-°F

@Temperature 100 °F
Maximum Service Temperature, Air 343 °C
650 °F
Fired Heaters
357 °C
675 °F
All Others
371 °C
700 °F
Film Temperature
Minimum Service Temperature, Air -10.6 °C
13.0 °F
start-up temp at 300 cPs
25.0 °C
77.0 °F
operating temp at 20 cPs
Pour Point <= -34.4 °C
<= -30.0 °F
D97