Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast ADHESIET 150 Dry Air-Setting Refractory Mortar Description: Adhesiet 150 is an air setting mortar with a sodium silicate bond and is supplied as a dry powder. Because of the special mix of the raw materials it can be used up to 1500°C.Remarks.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast AK 50 Dense Refractory Brick Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 53 E Dense Refractory Brick Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast CURON 150 AC Dense Refractory Castable Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast A 1 S Dense Refractory Brick Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Stellar Canada CERAMITE® CSA Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Continuous |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | No Load |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | No Load |
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Chosun Refractories 1500 ACE BLANKET Blanket Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | limited |
Chosun Refractories PT-150 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Carlisle 201LL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Anderman Ceramics EM80P Corundum Porous synthetic mullite with very high thermal shock. Available as tube, sheath, or rod up to 10 ft (3 m) long with diameters 0.3" to 20".Information provided by Anderman Ceramics. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Carlisle 201LD Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Maximum Service Temperature, Air | >= 1500 °C | >= 2730 °F | |
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | limited |
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Continuous |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Maximum Service Temperature, Air | >= 1500 °C | >= 2730 °F | |
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 45 Dense Refractory Brick Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av.. |