Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Pyrotek Grade 1250 Ceramic fiber paper Pyrotek Grade 1250 ceramic fiber paper is manufactured under carefully controlled conditions from high purity fibers to ensure close thickness tolerance and uniformity of density. The product conta.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast C Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast FI 25-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast... |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast C Sp Dense Refractory Brick Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Goodfellow Chromaloy O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Zircar Refractory Composites SIL-1 Silica Cloth ZIRCAR Type SIL Silica Cloths consists of high temperature non textured amorphous silica fiber yarn, woven into an extremely strong fabrics. These non preshrunk textiles are ideal for applications .. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Zircar Refractory Composites SIL-2 Silica Cloth ZIRCAR Type SIL Silica Cloths consists of high temperature non textured amorphous silica fiber yarn, woven into an extremely strong fabrics. These non preshrunk textiles are ideal for applications .. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Zircar Refractory Composites SIL-3 Silica Cloth ZIRCAR Type SIL Silica Cloths consists of high temperature non textured amorphous silica fiber yarn, woven into an extremely strong fabrics. These non preshrunk textiles are ideal for applications .. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Goodfellow Aluchrom O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Maximum Service Temperature, Air | >= 1250 °C | >= 2280 °F | |
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
BNZ Materials BNZP-23L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1250 °C | 2280 °F | |
Gouda Vuurvast FI 25-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |