Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 51981XA015 0.0150" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil PolyethyleneThis data r.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 910-10Rxx-P1 0.010" Cured, Self-Fusing Silicone Rubber 1.0 inch wide, 0.010" thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 920-10CxxFR-P1 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, brown, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 920-10Hxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.D.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 930-10Rxx-P1 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Static dissipating siliconeDesign/Construction:Interleave: 0.0025" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data repres.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon LW301Bxx-P0 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Des.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon LW40125B12-P0 0.040" Self-Fusing Silicone Rubber Tape 1.25 inches wide, 40 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in 12 yard long roll lengths.Design/Construction:Rubber: Cured Self-fusing Silicone R.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon R34710R020 0.020" Uncured Silicone Rubber with Mylar Carrier 20 mil thick, uncured, uncatalyzed silicone rubber. Used for sealing biochemical reaction chambers.Design/Construction:Liner: 3 mil Pink PEProduct: Uncured Silicone RubberCarrier: MylarThis data.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 44571XB015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate) Side 2: Uncured Silicone RubberInterleave: 2.5 mil .. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber 2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part num.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon T1012-R004-xx 0.012" Self-Fusing Silicone Rubber Tape 1 inch wide, 12 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, 12.0 yards long, red, triangular cross-section, self-fusing silicone tape.Design/Construction:Interleave: 1 mil PETProduct: Cured Silicone Self-fusing RubberCross-section.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 32570XA020 0.020" Uncured Silicone Rubber on Polyester Film Carrier Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |