Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 100 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax MF G Phenolic, Cotton Fabric Reinforcement, Black, Sheets Description: Exclusively for mechanical applications. Impact-resistant. Resistant to mechanical wear and noise-reducing. The graphite content causes low friction. Well suited for parts where there a.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets Description: Exclusively for mechanical applications. Impact-resistant, resistant to mechanical wear, noise-reducing, low friction. Well suited for parts where there are high mechanical load and wea.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing and wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environ.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax MFP G Phenolic, Cotton/synthetic Fabric Reinforcement, Black, Sheets Description: Exclusively for mechanical applications. The combination of cotton/synthetic reinforcement and a graphite-modified resin results in a material with low friction and especially high wear.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Reinforced with finer fabric than Etronax MF. Can be used, in particular, for mechanical applications where fine tolerances and smoother surface finish are requ.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environmen.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola Etronax MMMF PTFE Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets Description: Friction reducing material consisting of phenolic resin with PTFE (Teflon®) and a very fine cotton fabric. Exclusively for mechanical applications. Very good dry run properties. Well s.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola Etronax MF G Phenolic, Cotton Fabric Reinforcement, Black, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environmen.. |
|||
Maximum Service Temperature, Inert | 100 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
212 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola Etronax MFP G Phenolic, Cotton Fabric Reinforcement, Black, Tubes Description: Exclusively for mechanical applications. The combination of cotton/synthetic reinforcement and a graphite-modified resin results in a material with low friction and especially high wear.. |