Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Thermal Conductivity | 60.0 - 120 W/m-K | 416 - 833 BTU-in/hr-ft²-°F | |
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium Formall® 545 Aluminum Alloy Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Thermal Conductivity | 105 - 120 W/m-K | 729 - 833 BTU-in/hr-ft²-°F | |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
Thermal Conductivity | 20.0 - 120 W/m-K | 139 - 833 BTU-in/hr-ft²-°F | in "ab" direction |
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr.. |