Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.300 - 0.303 W/m-K | 2.08 - 2.10 BTU-in/hr-ft²-°F | Average value: 0.301 W/m-K Grade Count:3 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Thermal Conductivity | 0.190 - 0.303 W/m-K | 1.32 - 2.10 BTU-in/hr-ft²-°F | Average value: 0.281 W/m-K Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Thermal Conductivity | 0.170 - 0.303 W/m-K | 1.18 - 2.10 BTU-in/hr-ft²-°F | Average value: 0.258 W/m-K Grade Count:3 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |