Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 6.80 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.980 W/m-K
6.80 BTU-in/hr-ft²-°F
through-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compounding
Thermal Conductivity 0.980 W/m-K
6.80 BTU-in/hr-ft²-°F
ASTM C177
Techmer ES HiFill® PA4/6 0206
Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc.
Thermal Conductivity 0.980 W/m-K
6.80 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® EE149-6 Epoxy
Material Description: A single component, silver-filled, B-stageable epoxy designed for semiconductor flip chip packaging or hybrid micro-electronic substrate attach or lid-sealing.Information Provi..
Thermal Conductivity 0.980 W/m-K
6.80 BTU-in/hr-ft²-°F
through-plane, ø80*3mm discs; ISO 22007-2
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated