Polymer Property : Thermal Conductivity = 3.00 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity >= 0.432 W/m-K
>= 3.00 BTU-in/hr-ft²-°F
ASTM C177
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Thermal Conductivity >= 0.432 W/m-K
>= 3.00 BTU-in/hr-ft²-°F
ASTM C177
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Thermal Conductivity 0.432 W/m-K
3.00 BTU-in/hr-ft²-°F
ASTM F433
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide
Finished parts and basic shapes made from 15% by weight graphite filled polyimide material for applications high wear resistance, good thermal oxidative stability, and high temperature resistance. ..
Thermal Conductivity 0.432 W/m-K
3.00 BTU-in/hr-ft²-°F
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy
Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe..
Thermal Conductivity 0.432 W/m-K
3.00 BTU-in/hr-ft²-°F
ASTM C177
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle..
Thermal Conductivity >= 0.432 W/m-K
>= 3.00 BTU-in/hr-ft²-°F
ASTM C177
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.