Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.7 W/m-K | 206 BTU-in/hr-ft²-°F | |
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ.. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy sheet Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 0% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 10% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 10% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 20% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 20% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 30% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 30% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 40% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 40% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 40% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 40% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 50% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 30% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 29.7 W/m-K @Temperature 800 °C |
206 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |