Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.3 W/m-K @Temperature 300 °C |
113 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 400 °C |
113 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 400 °C |
113 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 400 °C |
113 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 400 °C |
113 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 400 °C |
113 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 301 Austenitic Stainless Steel, 1/2 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 301 Austenitic Stainless Steel, 1/4 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 301 Austenitic Stainless Steel, 1/8 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 301 Austenitic Stainless Steel, 3/4 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 301 Austenitic Stainless Steel, Annealed Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 301 Austenitic Stainless Steel, Full Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 302 Austenitic Stainless Steel, 1/2 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 302 Austenitic Stainless Steel, 1/4 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 302 Austenitic Stainless Steel, 1/8 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 302 Austenitic Stainless Steel, 3/4 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 302 Austenitic Stainless Steel, Full Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304 Austenitic Stainless Steel, 1/2 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304L Austenitic Stainless Steel, 3/4 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304L Austenitic Stainless Steel, Annealed Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304L Austenitic Stainless Steel, Full Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304 Austenitic Stainless Steel, 1/8 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304 Austenitic Stainless Steel, Annealed Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304 Austenitic Stainless Steel, Full Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304L Austenitic Stainless Steel, 1/2 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Thermal Conductivity | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | |
Eagle Brass 304L Austenitic Stainless Steel, 1/8 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 20.0 - 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800) AL 348 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 20.0 - 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100) AL 321 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Thermal Conductivity | 16.3 W/m-K @Temperature 20.0 - 100 °C |
113 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700) AL 347 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |