Thermal Properties Metric English Comments
Thermal Conductivity 0.159 W/m-K

@Temperature 205 °C
1.10 BTU-in/hr-ft²-°F

@Temperature 401 °F
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j..
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Dow Corning XIAMETER® PMCPPMX-200 10,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 10,000CS. 100% active, 10,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Dow Corning XIAMETER® PMCPPMX-200 350CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 350CS. 100% active, 350 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Dow Corning XIAMETER® PMCPPMX-200 5,000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 5,000CS. 100% active, high viscosity, polydimethylsiloxane polymer.Information provided by Dow Corning
Thermal Conductivity 0.159 W/m-K

@Temperature 50.0 °C
1.10 BTU-in/hr-ft²-°F

@Temperature 122 °F
Dow SPECFLEX™ NC 630 Polyol
SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082..
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Dow Corning 200® 1000 CST FLUID
100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Thermal Conductivity 0.159 W/m-K
1.10 BTU-in/hr-ft²-°F
Dow Corning XIAMETER® PMCPPMX-200 1000CS Silicone Fluid
Is chemically equivalent to DOW CORNING® 200 FLUID 1,000CS. 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning
Thermal Conductivity 0.159 W/m-K

@Temperature 100 °C
1.10 BTU-in/hr-ft²-°F

@Temperature 212 °F
Dow VORALUX™ HL 430 Copolymer Polyol
VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan..
Thermal Conductivity 0.159 W/m-K

@Temperature 50.0 °C
1.10 BTU-in/hr-ft²-°F

@Temperature 122 °F
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt..
Thermal Conductivity 0.159 - 0.187 W/m-K
1.10 - 1.30 BTU-in/hr-ft²-°F
Average value: 0.180 W/m-K Grade Count:4
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Thermal Conductivity 0.159 - 0.270 W/m-K
1.10 - 1.87 BTU-in/hr-ft²-°F
Average value: 0.211 W/m-K Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved