Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1026 Molded Foam Polyol Description: Pluracol® 1026 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams. HR foams made with Pluracol 1026 in combination with graft polyols.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1044 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1062 Specialty Polyol Description: Pluracol® 1062 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 1062 can also be use.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1135i Specialty Polyol Description: Pluracol® 1135i polyol is a nominal 1500 molecular weight triol. Pluracol 1135i has been prepared for applications in flexible slabstock foams and polyurethane adhesive and sealants ap.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1365 Graft Slabstock Foam Polyol Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 2086 Slabstock Foam Polyol Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 2097 Molded Foam Polyol Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 355 Specialty Polyol Description: Pluracol® 355 polyol is an amine-based tetrol of low equivalent weight with built-in catalytic activity. Because of its unusual behavior, this polyol has found wide application in flex.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 380 Specialty Polyol Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 4800 HR Foam Polyol Description: Pluracol® 4800 polyol is a primary OH tipped copolymer polyol containing approximately 45% copolymerized styrene-acrylonitrile suitable for molded foam applications. Pluracol polyol 48.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor p.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 593 Specialty Polyol Description: Pluracol® 593 polyol is a 3650 molecular weight polyol containing a high proportion of ethylene oxide in the polyol chain. Pluracol 593 can be used in the formulation for hydrophillic .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® GP 430R Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® P2010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® P710R Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® TP 2540 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® TP 740 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 2090 Specialty Polyol Description: Pluracol® 2090 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 2090 useful in the preparati.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 4156 Slabstock Foam Polyol Description: Pluracol® 4156 polyol is a 56 hydroxyl number (nominal 3000 molecular weight) polyether triol capable of producing a broad range of flexible slabstock polyurethane foams for furniture,.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 4600 Graft Slabstock Foam Polyol Description: Pluracol® 4600 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been form.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 4650 Graft Slabstock Foam Polyol Description: Pluracol® 4650 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been form.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 5250 Graft Slabstock Foam Polyol Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 628 Specialty Polyol Description: Pluracol® 628 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 628 can also be used .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® GP 730 Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® P1010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® TP 4040 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® TP 440 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Quadrol® Specialty Polyol Description: Quadrol® polyol is N, N, N´, N´-Tetrakis (2-hydroxypropyl) ethylene-diamine. Quadrol has proven to be an excellent cross-linking agent and catalyst for use in polyurethane coatings a.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1203 Specialty Polyol Description: Pluracol® 1203 is a conventional polyol with 2- and 3-functional characteristics. Pluracol1203 is specially designed for 1-component adhesives, foam-sealants, and microcellular elasto.. |
|||
Thermal Conductivity | 0.125 W/m-K | 0.868 BTU-in/hr-ft²-°F | |
BASF Pluracol® 1421 Molded Foam Polyol Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol.. |