Material Notes:
Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rigid polyurethane foams, coatings, adhesives, sealants and elastomers. Various members may be used in the preparation of prepolymers as cross-linking agents or as polyol reactants in one-shot systems.Information provided by BASF
Physical Properties Metric English Comments
Density 0.979 g/cc

@Temperature 60.0 °C
0.0354 lb/in³

@Temperature 140 °F
1.00 g/cc

@Temperature 37.8 °C
0.0361 lb/in³

@Temperature 100 °F
1.01 g/cc

@Temperature 25.0 °C
0.0365 lb/in³

@Temperature 77.0 °F
Viscosity 50 cP

@Temperature 60.0 °C
50 cP

@Temperature 140 °F
125 cP

@Temperature 37.8 °C
125 cP

@Temperature 100 °F
400 cP

@Temperature 25.0 °C
400 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.040
<= 0.040
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Composition Na & K
<7 ppm, STI 3038
Hydroxyl Number 61 - 67 mg KOH/g
STI 3007/3162