Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 9.80 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 20% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 40% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 40% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 50% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, hot rolled and 1050°C mill-annealed plate
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 1000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 16000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 4000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 4000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, plate, as annealed at 1025°C, rapid cooled
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Special Metals INCONEL® Alloy C-276
A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Special Metals INCONEL® C276 Nickel Superalloy Bar
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special ..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Special Metals INCONEL® C276 Nickel Superalloy Plate
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed)
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 30% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 40% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 50% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 50% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 10% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C (1500°F), good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a var..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 10% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Thermal Conductivity 9.80 W/m-K
68.0 BTU-in/hr-ft²-°F
RT
Haynes 625 alloy, 40% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Copyright © lookpolymers.com All Rights Reserved