Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.0 W/m-K @Temperature 1000 °C |
180 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Parker Chomerics C-Wing™ Heat Spreader Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. C-Wing spreaders are a cera.. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Momentive Performance Materials AC6043 Titanium Diboride/Boron Nitride Composite TiB2/BN. Density is 83-92% of theoretical. Sonic Modular1 is 4 to 17 x 10^6 psi.Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other r.. |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS292 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS296 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS303 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS304 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Goodfellow Nickel 70/Copper 30 Alloy Information provided by Goodfellow. |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Goodfellow Iron 90/Chromium 9/Molybdenum 1 Alloy High Chromium heat resistant ferritic steel with good weldability. Used for boiler tubesInformation provided by Goodfellow. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 95.0 °C |
180 BTU-in/hr-ft²-°F @Temperature 203 °F |
|
Crucible Steel AIRKOOL® (AISI A2) Tool Steel Airkool (AISI A2) is an air-hardening medium alloy tool steel which is heat treatable to HRC 60-62. It has wear resistance intermediate between the oil hardening tool steels (O1) and the high carbon.. |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 147-31N Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Thermal Conductivity | 26.0 W/m-K | 180 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Thermal Conductivity | 26.0 W/m-K @Temperature 20.0 - 100 °C |
180 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |