Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | x-y direction |
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | |
MarkeTech Mo70Cu Moly/Copper Heat Sink Material MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | |
MarkeTech W85Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | |
MarkeTech WCu15 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | z direction |
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
MMCC Aluminum/SiC 55p Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Thermal Conductivity | 190 W/m-K @Temperature 20.0 °C |
1320 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Kaiser 7068 T6, T6511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Thermal Conductivity | >= 190 W/m-K | >= 1320 BTU-in/hr-ft²-°F | |
H.C. Starck MoCu 70/30 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® 20X50 mesh Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® 50X100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® 50X80 mesh Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® GA95/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® M100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® M150 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® M80 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
TIMCAL TIMREX® 80X150 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® 3042 Silver Tungsten Carbide contact material ASTM B663 For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Thermal Conductivity | 190 W/m-K | 1320 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® 50S Infiltrated Tungsten Silver contact material ASTM B631, Class C, infiltrated For arcing and current carrying electrical contacts.Information provided by CMW Inc. |