Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMCAL TIMREX® M100 mesh FR Natural Flake Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® M100 mesh FR Natural Flake Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-des-Îles, Quebec, Canada. Further processing can be done either in Lac-des-Îles or for high added value products (e.g. TIMREX PG25) in our new processing plant in Terrebonne, Quebec, Canada. All TIMREX“Naturals” are thoroughly controlled in our laboratories to ensure quality, consistency and total customer satisfaction.Advantages and applications: Suitable for all organic bonded friction materials, especially for linings in drum brakes as well as in brake pads for trains. Good transfer film formationGood thermal conductivityExcellent lubricating properties Fe-self lubricating engineering parts Fe-friction partsCopper/bronze bearingsCopper friction parts copper clutch facings Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
Tap
Particle Size >= 75 µm
>= 75 µm
d50, 50%, vibrated sieving
>= 150 µm
>= 150 µm
d90, 7%, vibrated sieving
Deformation 1.2 %
1.2 %
elastic
5.2 %
5.2 %
plastic
6.4 %
6.4 %
plastic + elastic
Ash 4.0 - 6.0 %
4.0 - 6.0 %
Guaranteed
<= 7.0 %
<= 7.0 %
Thermal Properties Metric English Comments
Thermal Conductivity 190 W/m-K
1320 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Guaranteed
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Crystallite height Lc >350 nm
DBP absorption 42 g/100g
(Dibutylphthalate)