Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 19.8 W/m-K @Temperature 500 °C |
137 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 10% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 20% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 20% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 30% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 30% cold reduction, 1120°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 30% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 50% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 50% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, hot rolled and 1050°C mill-annealed plate Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 1000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 4000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, plate, as annealed at 1025°C, rapid cooled Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 19.8 W/m-K | 137 BTU-in/hr-ft²-°F | |
California Fine Wire Manganin 230 (Shunt) Copper, Manganese, and Nickel Resistance Wire All values may vary dependent on specific design and usageNickel content modifiedCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 30% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 30% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 50% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 50% cold reduction, 1120°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 10% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 10% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 19.8 W/m-K @Temperature 700 °C |
137 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 625 alloy, 40% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |