Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 0% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy sheet Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 20% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 30% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 50% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 30% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316 Austenitic Stainless Steel, 1/4 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316 Austenitic Stainless Steel, 1/8 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316 Austenitic Stainless Steel, 3/4 Hardened The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316L Austenitic Stainless Steel, 1/4 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316L Austenitic Stainless Steel, Annealed Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |