Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.5 W/m-K | 72.9 BTU-in/hr-ft²-°F | |
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.9 BTU-in/hr-ft²-°F | |
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.9 BTU-in/hr-ft²-°F | |
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.9 BTU-in/hr-ft²-°F | |
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.9 BTU-in/hr-ft²-°F | |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Thermal Conductivity | 10.5 - 10.8 W/m-K | 72.9 - 75.0 BTU-in/hr-ft²-°F | |
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92) Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.5 BTU-in/hr-ft²-°F | |
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.5 BTU-in/hr-ft²-°F | |
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.5 BTU-in/hr-ft²-°F | |
Ceradyne SEMICORE® S1-5C Specials SmCo5 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.5 BTU-in/hr-ft²-°F | |
Ceradyne SEMICORE® S2-17B MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.5 BTU-in/hr-ft²-°F | |
Ceradyne SEMICORE® S2-17C Specials Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.9 BTU-in/hr-ft²-°F | |
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Thermal Conductivity | 10.5 W/m-K | 72.5 BTU-in/hr-ft²-°F | |
Ceradyne SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |