Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.38 W/m-K | 9.58 BTU-in/hr-ft²-°F | in-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Thermal Conductivity | 1.38 W/m-K | 9.58 BTU-in/hr-ft²-°F | |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Thermal Conductivity | 1.38 W/m-K | 9.58 BTU-in/hr-ft²-°F | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Thermal Conductivity | 1.38 W/m-K | 9.57 BTU-in/hr-ft²-°F | |
Corning Vycor® 7913 UV-Transmitting Glass Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to high temperatures.Excellent thermal shock resistanceTypical Applications:Halogen l.. |
|||
Thermal Conductivity | 1.38 W/m-K | 9.57 BTU-in/hr-ft²-°F | |
Corning Vycor® 7950 Red Glass Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh.. |
|||
Thermal Conductivity | 1.38 W/m-K | 9.58 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |