Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.21 W/m-K | 8.40 BTU-in/hr-ft²-°F | |
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity. |
|||
Thermal Conductivity | 1.21 W/m-K | 8.41 BTU-in/hr-ft²-°F | COLORA |
Aptek 6550-A/B Epoxy Encapsulant High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for.. |
|||
Thermal Conductivity | 1.21 W/m-K | 8.40 BTU-in/hr-ft²-°F | |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Thermal Conductivity | 1.21 W/m-K | 8.40 BTU-in/hr-ft²-°F | ASTM C177 |
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass Polypropylene provides good resistance to acids, alkalis and organic solvents even at higher temperatures. It is, however, soluble in chlorinated hydrocarbons. Data provided by the manufacturer, Ow.. |