Polymer Property : Thermal Conductivity = 1.19 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.19 W/m-K
8.26 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E2116 is a two component, silver-filled and stencil printable electrically conductive adhesive for bonding SMDs onto PCB and substrates. Can be used as a “lead-free”..
Thermal Conductivity 1.19 W/m-K
8.26 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste
Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi..