Polymer Property : Thermal Conductivity = 0.870 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.870 W/m-K
6.04 BTU-in/hr-ft²-°F
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite
Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem..
Thermal Conductivity 0.870 W/m-K
6.04 BTU-in/hr-ft²-°F
ASTM D177
Manifattura Cattaneo VESPEL® SP21 Polyimide
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Thermal Conductivity 0.870 W/m-K

@Temperature 100 °C
6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
Thermal Conductivity 0.870 W/m-K
6.04 BTU-in/hr-ft²-°F
ASTM D5470
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon..